banner foundrie picture
Materials / Inox / Ferritique

EN(num.) 1.4002

General

Material category

Ferritique

Sectors of activity

Information

Caractéristiques de la norme EN 10250-4, ép. 25 mm max.\r\nTreatment recuit.

Features

C

0.08 max %

Si

1.00 max %

Mn

1.00 max %

P

0.040 max %

S

0.030 max %

Cr

12.00-14.00 %

Al

0.10-0.30 %

Rp0.2 min

230 min MPa

Rm min

400-600 MPa

Masse volumique

7.7 g/cm³

Equivalent standards

EN(num.)

1.4002, 1.4002

EN(sym.)

X6CrAl13, X6CrAl13

ISO

15510

NF

EN 10250-4

UNI

-

DIN

-

JIS

SUS 405, G4307

SAEASTM

-

UNS

-

BS

405S17

AFNOR

Z8CA12, NF A 35-573, Z6CA13-F, NF A 36-613

AISI

405

Autres

-