We use cookies to improve your browsing experience, but also to analyze our traffic. By clicking “Accept All”, you consent to our use of cookies.
We use cookies to help you navigate efficiently and perform certain features. You will find detailed information about all cookies under each consent category below.
We also use third-party cookies that help us analyze how you use this website. These cookies will only be stored in your browser with your prior consent.
You can choose to enable or disable some or all of these cookies, but disabling some of them may affect your browsing experience.
Material category
Austénitique
Sectors of activity
Caractéristiques de la norme EN 10250-4, forgés ép. 250 mm max.
C
0.030 max %
Si
1.00 mx %
Mn
2.00 max %
P
0.045 max %
S
0.030 max %
N
0.12-0.22 %
Cr
17.00-19.50 %
Ni
8.50-11.50 %
Rp0.2 min
270 min MPa
Rp0.2 max
0 MPa
Rm min
550-760 MPa
Rm max
0 MPa
A min
30 min transv %
Dureté max
0 HB
Résilience
min 100 long / 60 trans J
Masse volumique
8.0 g/cm³
EN(num.)
1.4311
EN(sym.)
X2CrNiN18-10, X2CrNiN18-10
ISO
ISO 4311-304-53-I
NF
EN10028-7, EN10088-3, EN10222-5, EN 10250-4
UNI
-
DIN
-
JIS
SUS 304LN
SAEASTM
A182 F304LN
UNS
S30453
BS
-
AFNOR
Z3CN18-10Az, NF A 35-573
AISI
304LN
Autres
AISI 304LN