We use cookies to improve your browsing experience, but also to analyze our traffic. By clicking “Accept All”, you consent to our use of cookies.
We use cookies to help you navigate efficiently and perform certain features. You will find detailed information about all cookies under each consent category below.
We also use third-party cookies that help us analyze how you use this website. These cookies will only be stored in your browser with your prior consent.
You can choose to enable or disable some or all of these cookies, but disabling some of them may affect your browsing experience.
Material category
Austénitique
Sectors of activity
Caractéristiques de la norme EN 10250-4, forgés ép. 250 mm max.
C
0.07 max %
Si
1.00 max %
Mn
2.00 max %
P
0.045 max %
S
0.030 max %
N
0.11 max %
Cr
16.50-18.50 %
Mo
2.00-2.50 %
Ni
10.00-13.00 %
Rp0.2 min
200 min MPa
Rp0.2 max
200 MPa
Rm min
500-700 MPa
Rm max
0 MPa
A min
30 min transv %
Dureté max
0 HB
Résilience
100 long / 60 transv min J
Masse volumique
8.0 g/cm³
EN(num.)
1.4401
EN(sym.)
X5CrNiMo17-12-2
ISO
-
NF
EN 10250-4, EN 10088-3
UNI
-
DIN
X5CrNi17-12, X5CrNi17-13, X8CrNi17-13
JIS
SUS 316, SUS 316 TP
SAEASTM
A182 F316, A240 316
UNS
S31600
BS
316 S 29, 316S 31, 316S 33, En58J
AFNOR
Z7 CND 17-11-02, Z7 CND 17-12-02, NF A 35-574, Z6CND17-12-F, NF A 36-613
AISI
316
Autres
AISI 316