Materials / Inox / Austénitique

EN(num.) 1.4429

Information

Caractéristiques de la norme EN 10250-4, forgés ép. 400 mm max.

Features

C

0.030 max %

Si

1.00 max %

Mn

2.00 max %

P

0.045 max %

S

0.015 max %

N

0.12-0.22 %

Cr

16.50-18.50 %

Mo

2.50-3.00 %

Ni

11.00-14.00 %

Rp0.2 min

280 min MPa

Rp0.2 max

0 MPa

Rm min

580-800 MPa

Rm max

0 MPa

A min

30 min transv %

Dureté max

0 HB

Résilience

100 long / 60 transv min J

Masse volumique

8.0 g/cm³

Equivalent standards

EN(num.)

1.4429

EN(sym.)

X2CrNiMoN17-13-3

ISO

-

NF

EN10028-7, EN10088-3, EN10222-5, EN10250-4

UNI

X2CrNiMoN17-13

DIN

-

JIS

SUS316LN

SAEASTM

A351 CF3MN

UNS

J92804, S31653 (5)

BS

316S63

AFNOR

Z3CND17-12Az, NF A 35-573, Z7CND18-12-03

AISI

316LN (5), 316LN