We use cookies to improve your browsing experience, but also to analyze our traffic. By clicking “Accept All”, you consent to our use of cookies.
We use cookies to help you navigate efficiently and perform certain features. You will find detailed information about all cookies under each consent category below.
We also use third-party cookies that help us analyze how you use this website. These cookies will only be stored in your browser with your prior consent.
You can choose to enable or disable some or all of these cookies, but disabling some of them may affect your browsing experience.
Material category
Superausténitique
Sectors of activity
Caractéristiques de la norme EN 10250-4, forgés avec ép. 250 mm max.
C
0.020 max %
Si
0.70 max %
Mn
1.00 max %
P
0.030 max %
S
0.010 max %
N
0.18-0.25 %
Cr
19.50-20.50 %
Mo
6.00-7.00 %
Ni
17.50-18.50 %
Cu
0.50-1.00 %
Rp0.2 min
300 min MPa
Rp0.2 max
260 MPa
Rm min
650-850 MPa
Rm max
450 MPa
A min
30 min transv %
Dureté max
0 HB
Résilience
100 long / 60 transv min J
Masse volumique
7.0 g/cm³
EN(num.)
1.4547
EN(sym.)
X1CrNiMoCuN20-18-7 (1)
ISO
-
NF
-
UNI
-
DIN
X1CrNiMoCuN20187 (1)
JIS
-
SAEASTM
A351 CK-3MCuN, A182 F44 (1)
UNS
J93254, S31254(1)
BS
-
AFNOR
Z1CNDU20-18-06 Az
AISI
-
Autres
254 SMO 6MO (B)