We use cookies to improve your browsing experience, but also to analyze our traffic. By clicking “Accept All”, you consent to our use of cookies.
We use cookies to help you navigate efficiently and perform certain features. You will find detailed information about all cookies under each consent category below.
We also use third-party cookies that help us analyze how you use this website. These cookies will only be stored in your browser with your prior consent.
You can choose to enable or disable some or all of these cookies, but disabling some of them may affect your browsing experience.
Material category
Austénitique
Sectors of activity
Caractéristiques de la norme EN 10250-4, forgés ép. 450 mm max.
C
0.08 max %
Si
1.00 max %
Mn
2.00 max %
P
0.045 max %
S
0.030 max %
Cr
16.50-18.50 %
Mo
2.00-2.50 %
Ni
10.50-13.50 %
Ti
5xC-0.70 %
Rp0.2 min
200 min MPa
Rp0.2 max
0 MPa
Rm min
500-700 MPa
Rm max
0 MPa
A min
30 min transv %
Dureté max
0 HB
Résilience
100 long / 60 transv min J
Masse volumique
8.0 g/cm³
EN(num.)
1.4571
EN(sym.)
X6CrNiMoTi17-12-2
ISO
-
NF
EN10028-7, EN10088-3, EN10222-5, EN10250-4
UNI
X6CrNiMoTi17-12
DIN
VdTUV 454, UNE F.3535, X10CrNiMoTi18-10
JIS
SUS 316Ti
SAEASTM
-
UNS
S31635
BS
320S17, 320S18, 320S31
AFNOR
Z6CNDT17-12-F, NF A 36-613, Z6CNDT17-12, NF A 35-574
AISI
316Ti, 316Ti
Autres
-