We use cookies to improve your browsing experience, but also to analyze our traffic. By clicking “Accept All”, you consent to our use of cookies.
We use cookies to help you navigate efficiently and perform certain features. You will find detailed information about all cookies under each consent category below.
We also use third-party cookies that help us analyze how you use this website. These cookies will only be stored in your browser with your prior consent.
You can choose to enable or disable some or all of these cookies, but disabling some of them may affect your browsing experience.
Material category
Alloyed steels
Sectors of activity
Processes used
Caractéristiques de la norme EN 10250-3 ép. 160-330 mm.
C
0.32-0.40 %
Si
0.40 max %
Mn
0.50-0.80 %
P
0.035 max %
S
0.035 max %
Cr
0.90-1.20 %
Mo
0.15-0.30 %
Ni
0.90-1.20 %
Rp0.2 min
500 min MPa
Rp0.2 max
0 MPa
Rm min
700 min MPa
Rm max
640 MPa
A min
15 min long %
Dureté min
250 typique HB
Dureté max
280 HB
Résilience
45 min long J
Masse volumique
7.86 g/cm³
EN(num.)
1.6511
EN(sym.)
36CrNiMo4
ISO
-
NF
-
UNI
-
DIN
39NiCrMo3
JIS
-
SAEASTM
-
UNS
-
BS
-
AFNOR
40NCD3
AISI
-