banner foundrie picture
Materials / Copper and alloy copper / Cupro-nickel Cu-Ni

ISO 204

General

Material category

Cupro-nickel Cu-Ni

Processes used

Features

Si

1 %

Ni

2 %

Cu

97 %

Rp0.2 min

320 MPa

Rp0.2 max

340 MPa

Rm min

450 MPa

Rm max

490 MPa

A min

8 %

A max

10 %

Dureté min

150 HB

Dureté max

160 HB

Résilience

0 J

Masse volumique

8.0 g/cm³

Equivalent standards

EN(num.)

-

EN(sym.)

-

ISO

204

NF

-

UNI

2528

DIN

17666

JIS

-

SAEASTM

C64700

UNS

-

BS

-

AFNOR

UN 2S

AISI

-

Autres

-