We use cookies to improve your browsing experience, but also to analyze our traffic. By clicking “Accept All”, you consent to our use of cookies.
We use cookies to help you navigate efficiently and perform certain features. You will find detailed information about all cookies under each consent category below.
We also use third-party cookies that help us analyze how you use this website. These cookies will only be stored in your browser with your prior consent.
You can choose to enable or disable some or all of these cookies, but disabling some of them may affect your browsing experience.
Material category
Alloyed steels
Sectors of activity
Processes used
Cr+Mo = 0.32 max.\r\nKV: test à -101°C, exigences 20/16 J pour LF3 class 1 et 27/20 J pour LF3 class 2.\r\nUtilisé pour des applications en cryogénie à -100°C
C
0.20 max %
Si
0.20-0.35 %
Mn
0.90 max %
P
0.035 max %
S
0.040 max %
Cr
0.30 max %
Mo
0.12 max %
Nb
0.02 max %
Ni
3.3-3.7 %
Cu
0.40 max %
V
0.03 max %
Rp0.2 min
260 min MPa
Rm min
485-655 MPa
A min
22 min %
A max
35 min %
Masse volumique
7.86 g/cm³
EN(num.)
-
EN(sym.)
-
ISO
-
NF
-
UNI
-
DIN
1.5639, 16Ni14, 1.5637, 12Ni14
JIS
-
SAEASTM
A350 LF3
UNS
-
BS
-
AFNOR
-
AISI
A2317
Autres
-