SAEASTM A494 N-12MV

Information

" '<p>Heat treatment (1) = S</p>\r\n<p>Microstructure (2) =&nbsp`£a, (i)</p>\r\n<p>Patternmaker\'s shrinkage = 1.8%</p>\r\n<p>Weldability (4) = 1</p>\r\n<p>&nbsp`£</p>\r\n<p><span style=\""text-decoration: underline`£\"">Legende</span></p>\r\n<p>(1) A: Annealed`£ N: Normalized and tempered`£ &nbsp`£H: Hardened and tempered`£ &nbsp`£S: Solution treated`£ &nbsp`£P: Precipitation hardened `£&nbsp`£</p>\r\n<p>(): &nbsp`£Optional.</p>\r\n<p>(2) a: Austenite`£ f: Delta ferrite`£ m: Martensite`£ i:Intermetallic phases`£ (): Secondary phase.</p>\r\n<p>(4) 1: Excellent`£ 2: Satisfactory`£ 3: Acceptable with precautions`£ 4: Usually unsatisfactory.</p>'"

Features

Fe

6.0 %

C

0.12 %

Cr

1.0 %

Mo

1.167 %

Ni

bal %

Rp0.2 min

275 MPa

Rp0.2 max

275 MPa

Rm min

525 MPa

Rm max

525 MPa

A min

6 %

A max

6 %

Dureté min

160 HB

Dureté max

240 HB

Résilience

40 J

Masse volumique

7.0 g/cm³

Equivalent standards

EN(num.)

2.4882

EN(sym.)

-

ISO

-

NF

-

UNI

-

DIN

GNiMo30

JIS

-

SAEASTM

A494 N-12MV

UNS

N30012, N10665 (5)

BS

-

AFNOR

-

AISI

-

Autres

Hastelloy� B-2 (5, 7)