We use cookies to improve your browsing experience, but also to analyze our traffic. By clicking “Accept All”, you consent to our use of cookies.
We use cookies to help you navigate efficiently and perform certain features. You will find detailed information about all cookies under each consent category below.
We also use third-party cookies that help us analyze how you use this website. These cookies will only be stored in your browser with your prior consent.
You can choose to enable or disable some or all of these cookies, but disabling some of them may affect your browsing experience.
Material category
Base Nickel
Sectors of activity
" '<p>Heat treatment (1) = `£S, P `£</p>\r\n<p>Microstructure (2) = `£a, (i)</p>\r\n<p>Patternmaker\'s shrinkage = 1.8%</p>\r\n<p>Weldability (4) = 2</p>\r\n<p> `£</p>\r\n<p>Dans les caracteristiques mecaniques, les valeurs min sont annoté`£es (S) et `£les valeurs max sont annoté`£es (P)</p>\r\n<p> `£</p>\r\n<p><span style=\""text-decoration: underline`£\"">Legende</span></p>\r\n<p>(1) A: Annealed`£ N: Normalized and tempered`£  `£H: Hardened and tempered`£  `£S: Solution treated`£  `£P: Precipitation hardened `£ `£</p>\r\n<p>():  `£Optional.</p>\r\n<p>(2) a: Austenite`£ f: Delta ferrite`£ m: Martensite`£ i:Intermetallic phases`£ (): Secondary phase.</p>\r\n<p>(4) 1: Excellent`£ 2: Satisfactory`£ 3: Acceptable with precautions`£ 4: Usually unsatisfactory.</p>'"
Fe
1.8 %
C
0 %
Cr
0.84 %
Mo
0.670 %
Ni
bal %
Rp0.2 min
290 MPa
Rp0.2 max
470 MPa
Rm min
575 MPa
Rm max
795 MPa
A min
18 %
A max
55 %
Dureté min
160 HB
Dureté max
260 HB
Résilience
50 J
Masse volumique
7.0 g/cm³