We use cookies to improve your browsing experience, but also to analyze our traffic. By clicking “Accept All”, you consent to our use of cookies.

Refuse all Accept all
banner foundrie picture
Materials / Cast iron GS and GL / GL

EN(num.) EN-GJL 300

General

Material category

GL

Processes used

Features

C

3,05 %

Si

1,75 %

Mn

0,95 %

Cr

0 %

Mo

0 %

Ni

0 %

Rp0.2 min

195 MPa

Rp0.2 max

260 MPa

Rm min

400 MPa

Rm max

450 MPa

A min

17 %

A max

17 %

Dureté min

0 HB

Dureté max

150 HB

Résilience

0 J

Masse volumique

7.1 g/cm³

Equivalent standards

EN(num.)

EN-GJL 300

EN(sym.)

-

ISO

-

NF

FT 30 A 32-101

UNI

G30 UNI 5007-69, EN 1561

DIN

-

JIS

-

SAEASTM

A278-85 CL 300

UNS

-

BS

-

AFNOR

-

AISI

-

Autres

-