We use cookies to improve your browsing experience, but also to analyze our traffic. By clicking “Accept All”, you consent to our use of cookies.

Refuse all Accept all
banner foundrie picture
Materials / Cast iron GS and GL / GS

EN(num.) EN GJS 350-22LT

General

Material category

GS

Processes used

Features

C

3,6 %

Si

1,9 %

Mn

<0,2 %

Cr

0 %

Mo

0 %

Ni

0 %

Rp0.2 min

220 MPa

Rp0.2 max

280 MPa

Rm min

450 MPa

Rm max

600 MPa

A min

20 %

A max

10 %

Dureté min

0 HB

Dureté max

220 HB

Résilience

0 J

Masse volumique

7.1 g/cm³

Equivalent standards

EN(num.)

EN GJS 350-22LT

EN(sym.)

-

ISO

-

NF

-

UNI

EN 1563

DIN

-

JIS

-

SAEASTM

A874-89

UNS

-

BS

370, 17

AFNOR

-

AISI

-

Autres

-