General

Material category

GS

Processes used

Features

C

3,6 %

Si

1,9 %

Mn

<0,2 %

Cr

0 %

Mo

0 %

Ni

0 %

Rp0.2 min

220 MPa

Rp0.2 max

280 MPa

Rm min

500 MPa

Rm max

500 MPa

A min

7 %

A max

7 %

Dureté min

170 HB

Dureté max

241 HB

Résilience

0 J

Masse volumique

7.1 g/cm³